    Getting ready to spray Duratec Vinylester Primer and it calls for "full strength mekP catalyst". The highest concentration mekP I can find is 50%, is this full strength? What catlyst should I be using?

    Thanks

  2. #2
    Join Date
    Jul 2006
    Posts
    1,137
    Thanks (Given)
    4
    Thanks (Received)
    57
    Likes (Given)
    124
    Likes (Received)
    224
    Mentioned
    1 Post(s)
    Tagged
    0 Thread(s)
    50% is fine. When a gel coat or Duratec calls for that type of catalyst it means do not use 40% or 45%. Tooling gels are the same way they call for 50% (hot) catalyst.
    Duratec gray sandable primer will call for 2% mix ratio but in hot weather that can be reduced to 1.5% with no problem.
    1970 15' Allison/135 Chrysler stacker
    RC Mod-VP Boats

    IMPBA District 13
    NAMBA District 3

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Frank Mole Transport